◆Place the glass on the heating platform.
◆Turn on the power and adjust the speed of roller.
◆Press “heating” button (pre-heating).
◆Tear any angle from polarizer about 50-80mm, attach conductive tape with one side and attach return tape with another side, place condutive tape onto roller.
◆Adjust motor to positive way and appropriate speed, then press ”start“ button and delaminating.
◆Delaminating finished, move away product.
◆Adjust motor to reverse direction and appropriate speed at the same time. Start the “material recycling” button to return scrap material.